Sign In | Join Free | My carsrow.com |
|
Brand Name : Zhonggong Special Metallurgy
Model Number : GH36 Alloy
Place of Origin : China
MOQ : 100KG
Price : Price is negotiated based on the required specifications and quantity
Payment Terms : Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability : 5000 tons per month
Delivery Time : 5-8 working days, depending on the parameters required for negotiation
Packaging Details : Standard export packaging, or packaging as required
Density : ~8.9 g/cm³ (0.321 lb/in³)
Melting Point : ~1350-1450°C (2460-2640°F)
Tensile Strength : ~850 MPa (123 ksi)
Yield Strength : ~700 MPa (102 ksi)
Elongation : ~15%
Thermal Conductivity : ~14 W/m·K (8.4 BTU·in/hr·ft²·°F)
Modulus of Elasticity : ~210 GPa (30 x 10³ ksi)
Corrosion Resistance : Good oxidation and corrosion resistance at high temperatures
Applications : Aerospace, gas turbines, and high-temperature structural components
Certification : ISO Certificate
GH36 Alloy is a high-performance nickel-based superalloy renowned for its exceptional mechanical properties and resistance to high-temperature environments. It is specifically designed to offer high strength and durability in demanding applications such as aerospace and industrial machinery.
Key Properties and Features:
High-Temperature Strength: GH36 Alloy maintains robust mechanical properties, including high tensile strength (~850 MPa or 123 ksi) and yield strength (~700 MPa or 102 ksi), at elevated temperatures up to approximately 1350-1450°C (2460-2640°F). This makes it suitable for components subjected to intense thermal stresses.
Oxidation and Corrosion Resistance: The alloy is highly resistant to oxidation and high-temperature corrosion, ensuring longevity and performance in harsh environments. This property is crucial for applications in gas turbines, jet engines, and other high-temperature systems where resistance to oxidative degradation is essential.
Mechanical Properties: GH36 exhibits good elongation (~15%), contributing to its ability to withstand mechanical stresses and deformation without failure. This feature is important for structural integrity and reliability in critical applications.
Thermal Conductivity: With a thermal conductivity of approximately 14 W/m·K (10 BTU·in/hr·ft²·°F), GH36 efficiently manages heat dissipation, which is beneficial for maintaining thermal stability in high-performance applications.
Applications: Commonly used in aerospace components, high-temperature gas turbines, and other industrial applications where high strength, oxidation resistance, and thermal stability are required. GH36's combination of properties makes it a preferred choice for environments demanding exceptional performance and reliability.
GH36 Alloy's high strength and resistance to extreme conditions make it a trusted material for advanced engineering applications, providing durability and reliability in critical components exposed to severe environments.
Here’s a composition table for GH36 Alloy:
Element | Composition Range (%) |
---|---|
Nickel (Ni) | 60.0 - 65.0 |
Chromium (Cr) | 15.0 - 20.0 |
Cobalt (Co) | 5.0 - 10.0 |
Molybdenum (Mo) | 2.0 - 4.0 |
Iron (Fe) | ≤ 6.0 |
Titanium (Ti) | 1.0 - 2.0 |
Aluminum (Al) | 1.0 - 2.0 |
Carbon (C) | ≤ 0.10 |
Manganese (Mn) | ≤ 0.5 |
Silicon (Si) | ≤ 0.5 |
Sulfur (S) | ≤ 0.01 |
These values provide general guidelines. For precise specifications or detailed applications, consult specific standards or suppliers.
![]() |
GH36 Alloy is a nickel-based superalloy with high strength and excellent oxidation resistance at elevated temperatures Images |